A mixed metal material that is recovered from MSW is further processed by using a magnetic binary separator that separates ferrous metals from non-ferrous metals. The mixed metal material enters the separator at a rate of 2.5 tons per day. Ferrous metal makes up 65% of this material. The product recovery stream leaves the separator at a rate of 1.75 tons per day with 88% of that being ferrous metals. The remainder of the material leaves the separator in the material reject stream.
a) Calculate the percent of ferrous metal recovery
b) Calculate the purity of the ferrous metal in the product recovery stream
c) Calculate the overall efficiency of the separator
a) Calculate the percent of ferrous metal recovery
b) Calculate the purity of the ferrous metal in the product recovery stream
c) Calculate the overall efficiency of the separator
Answers
Related Questions
A few clips made of magnetic material are placed in a container and a magnet attracts the clips from...
In a certain material for which µ = 6.5 o
,
H = 10ax + 25ay - 40az A/m
Find (a) The magnetic...
A phenomenon where a magnetic material temporarily
acquires magnetic properties when a magnet is br...
When an object that is made of magnetic material but is not a magnet comes in contact with a magnet...